Plastic Ladder Ring packing flange lateral side increased, not only can increase the mechanical strength of packing rings, and because of damage to the packing structure of the axis of symmetry, thus increasing the chance of filling the orientation when released. Also, because the flanging effect, making the filling in the gaps between the stacked packing rings when the contact becomes dominated by the linear contact with a point of contact. This will not only increase the gap between the filler particles, reducing the gas through the packing layer of negative forces, and these contacts can also fill the surface of the liquid flows along the scattered points of convergence, thus contributing to the film surface update conducive to packing mass transfer efficiency.
Specification:
Diameter (mm) | Size (mm) | Surface Area (m2/m3) | Void Rate (m3/m3) | Number PCE/M3 | Weight Kg/M3 | Dry Packing Factor (m-1) |
Ф16 | 16x8x1.0 | 346 | 0.85 | 134 | 297000 | 563 |
Ф25 | 25×13×1.2 | 214 | 0.91 | 81 | 81000 | 284 |
Ф38 | 38×19×1.2 | 172 | 0.93 | 62 | 27000 | 214 |
Ф50 | 50×25×1.5 | 121 | 0.93 | 62 | 10700 | 150 |
Ф76 | 76×38×2.5 | 84 | 0.93 | 63 | 3400 | 104 |